MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hifax ETA4161U P23494 J DEERE GRY Thermoplastic Polylefinic
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax ETA4161U P23494 J DEERE GRY fractional melt flow, medium flexural modulus, thermoplastic polyolefin (TPO) is typically used as a cap layer for interior and exterior applications that require good scratch and mar resistance and can improve stress whitening issues. This extrusion grade material exhibits enhanced melt strength for a wide thermoforming process window.

Status: Commercial - Active

Availability: North America

Application: Industrial; Panels & Profiles

Market: Automotive

Processing Method: Injection Molding

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183-1
Melt Flow 0.600 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.600 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.0 MPa4060 psi50 mm/min; ISO 527-1, -2
Flexural Modulus 1.15 GPa167 ksi2 mm/min; ISO 178
Impact Test 23.0 J17.0 ft-lbMulti-axial, 2.2 m/s, 3.2 mm plaque, Energy at Peak Force, Ductile Behavior; ASTM D3763

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9116 / 324051

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.