MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Expanded Polystyrene (EPS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.00310 - 3.50 g/ccAverage value: 0.212 g/cc Grade Count:385
Filler Content 0.300 - 10.5 %Average value: 5.17 % Grade Count:37
Water Absorption 0.0300 - 9.00 %Average value: 0.397 % Grade Count:50
Particle Size 100 - 3150 µmAverage value: 983 µm Grade Count:95
Water Vapor Transmission 50.0 - 200 g/m²/dayAverage value: 126 g/m²/day Grade Count:6
Viscosity 1.65 - 1.70 cPAverage value: 1.67 cP Grade Count:9
Permeability 0.500 - 3.50Average value: 1.79 Grade Count:19
Maximum Moisture Content 0.200 - 0.500Average value: 0.403 Grade Count:40
Melt Flow 1.80 - 4.00 g/10 minAverage value: 2.53 g/10 min Grade Count:3
Outgassing - Total Mass Loss 1.00 - 2.50 %Average value: 1.39 % Grade Count:7
Vapor Pressure 0.685 barAverage value: 0.685 bar Grade Count:9
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 0.0800 - 1.10 MPaAverage value: 0.464 MPa Grade Count:47
Tensile Strength, Yield 47.1 - 51.0 MPaAverage value: 48.4 MPa Grade Count:3
Elongation at Break 5.00 - 13.4 %Average value: 8.45 % Grade Count:21
Creep Strength 0.0600 - 0.300 MPaAverage value: 0.156 MPa Grade Count:6
Modulus of Elasticity 0.00650 - 2.65 GPaAverage value: 0.484 GPa Grade Count:8
Flexural Yield Strength 0.0750 - 3.00 MPaAverage value: 0.433 MPa Grade Count:142
Flexural Modulus 0.00628 - 0.0342 GPaAverage value: 0.0153 GPa Grade Count:20
Flexural Strain at Break 6.90 - 14.1 %Average value: 10.8 % Grade Count:16
Compressive Yield Strength 0.0392 - 10.9 MPaAverage value: 0.461 MPa Grade Count:156
Compressive Modulus 0.00500 - 0.0400 GPaAverage value: 0.0177 GPa Grade Count:6
Shear Strength 0.200 - 0.300 MPaAverage value: 0.290 MPa Grade Count:5
Adhesive Bond Strength 0.100 - 0.400 MPaAverage value: 0.165 MPa Grade Count:5
Izod Impact, Notched 0.216 - 0.245 J/cmAverage value: 0.235 J/cm Grade Count:3
Puncture Energy 41.4 - 316 JAverage value: 103 J Grade Count:16
Tear Strength 1.05 - 6.10 kN/mAverage value: 2.74 kN/m Grade Count:17
K Factor (Wear Factor) 54.0 - 59.0Average value: 56.8 Grade Count:13
Compression Set 32.2 - 45.7 %Average value: 41.1 % Grade Count:20
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+10 - 1.00e+12 ohmAverage value: 2.44e+11 ohm Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 - 80.0 µm/m-°CAverage value: 66.3 µm/m-°C Grade Count:33
CTE, linear, Transverse to Flow 60.0 µm/m-°CAverage value: 60.0 µm/m-°C Grade Count:6
Thermal Conductivity 0.0270 - 0.0450 W/m-KAverage value: 0.0353 W/m-K Grade Count:106
 0.0240 - 0.0370 W/m-K
@Temperature -80.0 - 50.0 °C
Average value: 0.0312 W/m-K Grade Count:5
 0.0240 - 0.0370 W/m-K
@Temperature -80.0 - 50.0 °C
Average value: 0.0312 W/m-K Grade Count:1
 0.0240 - 0.0370 W/m-K
@Thickness 50.0 - 50.0 mm
Average value: 0.0312 W/m-K Grade Count:1
Insulation R Value 3.66 - 20.0Average value: 8.05 Grade Count:7
 >= 5.40
@Temperature -3.89 - 4.44 °C
Average value: 9.35 Grade Count:3
 >= 5.40
@Thickness 25.4 - 76.2 mm
Average value: 9.35 Grade Count:3
Maximum Service Temperature, Air 70.0 - 118 °CAverage value: 83.7 °C Grade Count:53
Vicat Softening Point 99.0 - 104 °CAverage value: 101 °C Grade Count:3
Softening Point 70.0 °CAverage value: 70.0 °C Grade Count:26
Decomposition Temperature 220 °CAverage value: 220 °C Grade Count:26
Flame Spread 1.20 - 136 mm/minAverage value: 53.6 mm/min Grade Count:13
Flash Point -56.0 °CAverage value: -56.0 °C Grade Count:26
Ignition Temperature 285 °CAverage value: 285 °C Grade Count:26
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90.0 %Average value: 90.0 % Grade Count:3
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.500 - 3.00 %Average value: 1.06 % Grade Count:37

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Impact Modified
Overview of materials for Polystyrene, Extrusion Grade
Overview of materials for Polystyrene, Molded, Unreinforced
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe)
BASF Peripor® 200 Expandable Polystyrene

O4850 / 78420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.