MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® P-63P PFA Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Fluon® PFA (perfluoroalkoxy) is a melt-processible copolymer of tetrafluoroethylene and a perfluorinated vinyl ether. Fluon® PFA has chemical, electrical, and thermal properties almost identical to its close chemical cousin, polytetrafluoroethylene (PTFE), yet can be processed by conventional extrusion, injection molding, blow molding, and transfer molding techniques. This material can be used over a wide range of temperatures (-200°C to 260°C). It is available as a 1/8” pellet.

Benefits:

  • High Resistance to Heat
  • Excellent Chemical Resistance
  • Low Smoke and Flame Characteristics. Fluon® PFA is rated 94V-0 by Underwriters Laboratories Inc.
  • Outstanding Resistance to Weather and Aging
  • Excellent Dielectric Properties
  • Non-Stick Characteristics
Applications:
  • Tubing and Pipe
  • Film and Sheets
  • Valves, Fittings, and Housings
  • Wire and Cable

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.14 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
Melt Flow 12 g/10 minASTM D3159
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength 8.96 MPa
@Temperature 250 °C
ASTM D638
 32.0 MPa
@Temperature 23.0 °C
ASTM D638
 50.0 MPa
@Temperature -79.0 °C
 110 MPa
@Temperature -129 °C
 140 MPa
@Temperature -198 °C
Elongation at Break 1.0 %
@Temperature -198 °C
 1.0 %
@Temperature -129 °C
 9.0 %
@Temperature -79.0 °C
 410 %
@Temperature 23.0 °C
ASTM D638
 600 %
@Temperature 250 °C
ASTM D638
Flexural Strength 2.50 MPa
@Temperature 250 °C
ASTM D790
 8.00 MPa
@Temperature 100 °C
ASTM D790
 19.0 MPa
@Temperature 25.0 °C
ASTM D790
Flexural Modulus 20.0 MPa
@Temperature 250 °C
ASTM D790
 180 MPa
@Temperature 100 °C
ASTM D790
 630 MPa
@Temperature 25.0 °C
ASTM D790
 1600 MPa
@Temperature -79.0 °C
 4000 MPa
@Temperature -129 °C
Flex Crack Resistance 25000Cycles per MIT Folding Endurance; ASTM D2176
Izod Impact, Notched 680 J/m
@Temperature -40.0 °C
ASTM D256
 NB
@Temperature 23.0 °C
ASTM C256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Dielectric Constant 2.07
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 74.8 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µin/in-°F
@Temperature 0.000 - 100 °C
ASTM D696
 >= 90.0 µm/m-°C
@Temperature -100 - -75.0 °C
ASTM D696
 >= 110 µm/m-°C
@Temperature -75.0 - -15.0 °C
ASTM D696
 >= 140 µm/m-°C
@Temperature -15.0 - 100 °C
ASTM D696
 >= 160 µm/m-°C
@Temperature 100 - 150 °C
ASTM D696
 >= 210 µm/m-°C
@Temperature 150 - 210 °C
ASTM D696
Specific Heat Capacity 1.05 J/g-°C
Melting Point 310 °CASTM D3459
Maximum Service Temperature, Air 260 °C
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °CASTM D648
Vicat Softening Point 281 °C50°C/h; JIS K7206
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.35ASTM D542
 
Descriptive Properties
Heat of Combustion2200 BTU/lbASTM D240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® P-66P PFA Resin
AGC Fluon® P-65P PFA Resins
AGC Fluon® P-62XP PFA Resin
AGC Fluon® C88AXMP-HT ETFE
AGC Fluon® C-88AXMP ETFE

PAGCX259 / 191368

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.