MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. The product has been specifically designed for the production of refrigerator part: inner liners, door liners. injected parts etc.

This grade is also proposed for the production of packaging intended for products likely to cause stress cracking e.g. fats, oil...

POLYSTYRENE IMPACT 8260 retains good mechanical properties at low temperatures making this grade suitable for frozen packaging; it also affords good printing performance.

Applications Sheet for thermoforming, fridge liners, low temperature packaging applications (ice cream boxes and lids), packaging for aggressive foodstuffs, matte finish, soft touch.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 2.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133 H
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaISO 527-2
Tensile Strength, Yield 20.0 MPaISO 527-2
Elongation at Break >= 60 %ISO 527-2
Tensile Modulus 1600 MPaISO 527-2
Flexural Modulus 1600 MPaISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+13 ohmISO IEC 93
Dielectric Strength 150 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 91.0 µm/m-°C
Vicat Softening Point 90.0 °C
@Load 5.10 kg
50°C per hour; ISO 306B50
 99.0 °C
@Load 1.02 kg
50°C per hour; ISO 306A50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene
Overview of materials for Polystyrene, Molded, Unreinforced
SSAB Tunnplat Docol® DC04 (Fe P04) Deep-drawing Steel
SSAB Tunnplat Docol® DC01 (Fe P01) Deep-drawing Steel
Parkway Products Thixomolded® AM50A Magnesium

PTOTAL883 / 130608

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.