MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
LATI Laticonther 52/35 CP1/45 PP Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Linear Mold Shrinkage, Flow 0.010 - 0.013 cm/cm
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22.0 MPa
Elongation at Break 1.2 %
Tensile Modulus 3400 MPa
Charpy Impact Unnotched 5.00 kJ/m²
Charpy Impact, Notched 2.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+12 ohm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 3.50 W/m-KLongitudinal
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
Vicat Softening Point 100 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 250 °C
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Total PPH 12020 Polypropylene Homopolymer, Injection Molding
Techmer ES HiFill® PP 0123 C Polypropylene
RTP Company RTP 199 X 104849 A Polypropylene (PP), Thermally Conductive - Electrically Conductive
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass

PLATH9796 / 177492

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.