LATI Laticonther 52/35 CP1/45 PP Homopolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.23
g/cc
0.0444
lb/in³
Linear Mold Shrinkage, Flow
0.010
-
0.013
cm/cm
0.010
-
0.013
in/in
Linear Mold Shrinkage, Transverse
0.0095
-
0.0125
cm/cm
0.0095
-
0.0125
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
22.0
MPa
3190
psi
Elongation at Break
1.2 %
1.2 %
Tensile Modulus
3.40
GPa
493
ksi
Charpy Impact Unnotched
0.500
J/cm²
2.38
ft-lb/in²
Charpy Impact, Notched
0.200
J/cm²
0.952
ft-lb/in²
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+12
ohm
1.00e+12
ohm
Thermal Properties
Metric
English
Comments
Thermal Conductivity
3.50
W/m-K
24.3
BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi)
120
°C
248
°F
Deflection Temperature at 1.8 MPa (264 psi)
90.0
°C
194
°F
Vicat Softening Point
100
°C
@Load 5.00 kg
212
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
230
-
250
°C
446
-
482
°F
Mold Temperature
20.0
-
40.0
°C
68.0
-
104
°F
Drying Temperature
80.0
-
90.0
°C
@Time 10800 sec
176
-
194
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Total PPH 12020 Polypropylene Homopolymer, Injection Molding
Techmer ES HiFill® PP 0123 C Polypropylene
RTP Company RTP 199 X 104849 A Polypropylene (PP), Thermally Conductive - Electrically Conductive
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass
PLATH9796 / 177492
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.