MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

NOVA Chemicals NOVAPOL® LA-0522-A LDPE Extrusion Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes:

Homopolymer

Features:

  • Excellent sealability
  • High drawdown
  • High adhesion
  • Good foam processing window
  • Maintains foam dimensional stability
  • Achieves packaging foam density

Additives:

  • Base resin

Applications:

  • Paperboard containers
  • Woven fabrics
  • Lumber wrap
  • Foam plank
  • Foam sheetingBlending resin

United States: NOVAPOL LA-0522-A resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.1, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D 792
Water Vapor Transmission 17.0 g/m²/day
@Temperature 38.0 °C
1.09 g/100 in²/day
@Temperature 100 °F
Moisture Vapor Transmission Rate, 38°C (100°F), 90% RH on 30 lb Kraft paper samples with a LDPE coating weight of 15 lb/ream.; ASTM F 1249
Melt Index of Compound 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Neck In 5.10 cm2.01 in@ 1000 ft/min; total of both sides; NOVA Chemicals test method
Drawdown 8.10 m/s1590 ft/minNOVA Chemicals test method
Coating Weight >= 8.00 g/m²>= 5.00 lb/reamTAPPI D 539
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 9.40 MPa1360 psiASTM D 638
Elongation at Break 650 %650 %ASTM D 638
Flexural Modulus, 1% Secant 276 MPa40000 psiASTM D 790
Hot Tack Strength 225 g/25 mm
@Temperature 38.0 °C
225 g/in
@Temperature 100 °F
90% RH on 30 lb Kraft paper samples with a LDPE coating weight of 15 lb/ream.
Heat Seal Strength 1400 g/25 mm
@Temperature 38.0 °C
3.09 lb/in
@Temperature 100 °F
90% RH on 30 lb Kraft paper samples with a LDPE coating weight of 15 lb/ream.; TAPPI D517
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Braskem BC818 Extrusion Coating Low Density Polyethylene
Carmel Olefins Ipethene® 111 Low Density Polyethylene

PNOVB003 / 194611

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.