MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Unitemp 212 Iron-Nickel Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: High-strength alloy. Mechanical property data for solution treated + aged samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Rupture Strength 42500 psi
@Temperature 732 °C,
Time 3.60e+6 sec
 63000 psi
@Temperature 732 °C,
Time 360000 sec
 88000 psi
@Temperature 649 °C,
Time 3.60e+6 sec
 100000 psi
@Temperature 649 °C,
Time 360000 sec
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0290 cal cm/sec-cm²-°C
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.15 %
Boron, B 0.060 %
Carbon, C 0.080 %
Chromium, Cr 16 %
Iron, Fe 53.96 %Balance
Manganese, Mn 0.050 %
Nickel, Ni 25 %
Niobium, Nb (Columbium, Cb) 0.50 %
Silicon, Si 0.15 %
Titanium, Ti 4.0 %
Zirconium, Zr 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Invar® Controlled Expansion Alloys Iron-Nickel Alloys
Aperam FeNi 70 Controlled Expansion Alloys Iron-Nickel Alloys
Armco 20-45-5 Iron-Nickel Alloy
S-590 Iron-Nickel Alloy
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy

NZ97063 / 191460

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.