MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unitemp 212 Iron-Nickel Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: High-strength alloy. Mechanical property data for solution treated + aged samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.92 g/cc0.286 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  293 MPa
@Temperature 732 °C,
Time 3.60e+6 sec
42500 psi
@Temperature 1350 °F,
Time 1000 hour
 434 MPa
@Temperature 732 °C,
Time 360000 sec
63000 psi
@Temperature 1350 °F,
Time 100 hour
 607 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
88000 psi
@Temperature 1200 °F,
Time 1000 hour
 689 MPa
@Temperature 649 °C,
Time 360000 sec
100000 psi
@Temperature 1200 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 12.1 W/m-K
@Temperature 20.0 - 100 °C
84.1 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.15 %0.15 %
Boron, B 0.060 %0.060 %
Carbon, C 0.080 %0.080 %
Chromium, Cr 16 %16 %
Iron, Fe 53.96 %53.96 %Balance
Manganese, Mn 0.050 %0.050 %
Nickel, Ni 25 %25 %
Niobium, Nb (Columbium, Cb) 0.50 %0.50 %
Silicon, Si 0.15 %0.15 %
Titanium, Ti 4.0 %4.0 %
Zirconium, Zr 0.050 %0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam Invar® Controlled Expansion Alloys Iron-Nickel Alloys
Aperam FeNi 70 Controlled Expansion Alloys Iron-Nickel Alloys
Armco 20-45-5 Iron-Nickel Alloy
S-590 Iron-Nickel Alloy
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy

NZ97063 / 191460

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.