MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Allyl alcohol, C3H6O
Categories: Fluid; Solvent

Key Words: C3H6O
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.855 g/cc
@Temperature 20.0 °C
0.0309 lb/in³
@Temperature 68.0 °F
Viscosity 1.331 cP
@Temperature 20.0 °C
1.331 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 58.08 g/mol58.08 g/mol
Vapor Pressure 0.022563 bar
@Temperature 20.0 °C
16.924 torr
@Temperature 68.0 °F
Surface Tension 27.53 dynes/cm
@Temperature 20.0 °C
27.53 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 57.1 bar42900 torr
Critical Temperature 272 °C522 °F
Critical Density 0.286 g/cc0.0103 lb/in³
Critical Molar Volume 203 cm³/mol12.4 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 19.7
@Temperature 20.0 °C
19.7
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 688 J/g296 BTU/lb
Specific Heat Capacity 1.309 J/g-°C
@Temperature 25.0 °C
0.3129 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1574 W/m-K
@Temperature 20.0 °C
1.092 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -129.2 °C-200.6 °F
Boiling Point 96.9 °C206 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.411
@Wavelength 589.3 nm
1.411
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.9066
Antoine's Vapor Pressure B Parameter2928.2
Antoine's Vapor Pressure C Parameter-85.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)107-18-6
Chemical FormulaC3H6O
Critical Compressibility (Zc)0.256
Dipole moment (p/C.m)none
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A793.52
Dynamic Viscosity Parameter B307.26
Henry's Law Constant (atm m3/mol)6.2E-06
Molar Heat Capacity (298K)76.002 J/mol-K
Molar Heat Capacity of Vapor a Parameter-1.1046
Molar Heat Capacity of Vapor b Parameter0.3144
Molar Heat Capacity of Vapor c Parameter-0.000203
Molar Heat Capacity of Vapor d Parameter5.318E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1098

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VORANOL™ CP 6001 Polyol
ChevronTexaco Superla® 5 White Oil
Solvay RHODASURF® AAE-10 Surfactant
Solvay RHODASURF® AAE-10 E Surfactant
Solvay RHODAPEX® CO-436 Surfactant

VORGS011 / 99405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.