MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAPEX® CO-436 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: AMMONIUM NONYLPHENOL ETHER SULFATE

CAS: 68649-55-8

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAPEX CO-436 can be used to prepare a broad range of commercial emulsion polymers including acrylics, vinyl-acrylics, and styrene-acrylics. Such polymers find application in latex paints, adhesives, paper coatings, and textiles. RHODAPEX CO-436 is particularly useful in the preparation of small particle size emulsion polymers with high water resistance and excellent chemical stability. The versatility of RHODAPEX CO-436 allows it to be used with a wide range of polymerization techniques. Including thermal and redox processes. When properly used in conjunction with other anionic and nonionic surfactants, RHODAPEX CO-436 allows fro the trouble-free commercial production of extremely stable emulsion polymers.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 58 %58 %
 60 - 64 %
@Temperature 105 °C,
Time 7200 sec
60 - 64 %
@Temperature 221 °F,
Time 2.00 hour
Oven; RP-0540
pH 6.5 - 7.56.5 - 7.510% Solution; RP-0420
Surface Tension 33 dynes/cm33 dynes/cmat CMC
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Fe (Iron) <= 5.0 ppm<= 5.0 ppmO-Phenanthroline; RP-0277
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 5.0<= 5.0RPG-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 20 - 25 %20 - 25 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClean, Clear liquidRP-0064
CompositionActive58-60%, EQ. WT. 504, RP-0026
 Ethanol12-16%, RP-0181
Critical Micelle Concentration (%)0.03
Ionic ChargeAnionic
OdorAlcoholicRP-0359

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAPEX® AB 20 Surfactant
Solvay RHODAPEX® CD-128 Surfactant
Solvay RHODAPEX® EA-2 Surfactant
Solvay RHODAPEX® ES-2/K Surfactant
Solvay RHODAPEX® EST-30/BLB Surfactant

WRHOD377 / 137608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.