MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processability and clarity. Skygreen® PETG provides a material having outstanding toughness, clarity, color, chemical resistance, and resistance to stress whitening. It can readily be thermoformed for extrusion blow molded. It is superior to acrylic for toughness, and superior to polycarbonate for processability.

Applications: Extrusion Sheet: architecture protective cover, display signs, industrial products. Extrusion Film: blister packaging, food packaging containers, electrical & electronic packaging, pharmaceutical & medical packaging. Injection Molding: toys, refrigerator parts, electric & electronic parts, smart cards, pen caps, medical devices and tools. Extrusion Blow Molding: bottles for cosmetics, soaps, shampoos, detergents, etc.

Information provided by SK Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Water Absorption 0.13 %24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength at Break 28.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa50 mm/min; ASTM D638
Elongation at Break 140 %50mm/min; ASTM D638
Flexural Strength 73.0 MPa1.27 mm/min; ASTM D790
Flexural Modulus 2.10 GPa1.27 mm/min; ASTM D790
Izod Impact, Notched 100 J/mASTM D256
Impact Test 33.0 J
@Thickness 3.20 mm
impact resistance energy, max. load in plaque, 220 m/min; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 2.4
@Frequency 1e+6 Hz
ASTM D150
 2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mmshort-time, 500v/sec; ASTM D149
Dissipation Factor 0.0050
@Frequency 1000 Hz
ASTM D150
 0.023
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CASTM D648
Vicat Softening Point 85.0 °Cat 1 kg load; ASTM D1525
Glass Transition Temp, Tg 80.0 °CDSC
Flammability, UL94 HB
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 45.0 °CRoll 1 Temperature
 54.0 °CRoll 2 Temperature
 63.0 °CRoll 3 Temperature
 210 °CCylinder 4 Temperature
 245 °CCylinder 2 and Cylinder 3 Temperature
 245 °CScreen, Me1t Pump, and Connection Temperature
Feed Temperature 240 °C
Nozzle Temperature 245 °C
Zone 1 356 °FBarrel Temp of Main Extruder
 383 °FExtrusion Blow Molding
Zone 2 410 °FExtrusion Blow Molding
 473 °FBarrel Temp of Main Extruder
Zone 3 410 °FExtrusion Blow Molding
 509 °FBarrel Temp of Main Extruder
Zone 4 410 °FExtrusion Blow Molding
 500 °FBarrel Temp of Main Extruder
Zone 5 464 °FBarrel Temp of Main Extruder
Adapter Temperature 200 °CExtrusion Blow Molding
 245 °C
Die Temperature 383 °FExtrusion Blow Molding (Die Tip)
 477 °FDie Zone 1
 480 °FDie Zone 2
Head Temperature 185 °CExtrusion Blow Molding
Mold Temperature 12.0 - 20.0 °CExtrusion Blow Molding
 40.0 °C
 40.0 - 70.0 °CFor Thermoforming (Forming time = 3-10 sec)
Drying Temperature 65.0 °C
Dry Time 6 - 12 hour
Injection Pressure 5.50 MPa1st Pressure
Hold Pressure 4.00 MPa
 8.30 MPaExtrusion Melt Pressure
Back Pressure 0.500 MPa
Cycle Time - Injection 2.0 sec
 15 sec2nd Pressure Time
Cycle Time - Cooling 15 sec

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Eastar 6763 PETG Copolyester
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin
Eastman Tritan™ MX810 Medical Grade Copolyester
Eastman PROVISTA Copolymer PETG Copolyester
Overview of materials for PETG Copolyester

PSK000 / 67735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.