MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman PROVISTA Copolymer PETG Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Color, b* CIELAB, Illuminant D6500, 10° Observer is 0.61 per ASTM D 2244.

PROVISTA Copolymer is a resin specifically developed for extrusion into profiles where aesthetics like high clarity and gloss, coupled with design flexibility drive demand. Compared to commonly used materials, PROVISTA copolymer can often run on most standard processing equipment at increased speeds. An extremely high melt strength makes the resin an excellent choice when extruding profiles into complicated shapes.

Applications: Candy packaging; Food packaging; Furniture guards; Point of purchase displays; Pricing channels; Teething rails; Tubing

Properties reported here are based on limited testing. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.

Information provided by Eastman Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Ultimate 29.0 MPa4210 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 109 %109 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Flexural Yield Strength 72.0 MPa10400 psiASTM D790
Flexural Modulus 2.20 GPa319 ksiASTM D790
Izod Impact, Notched 0.940 J/cm1.76 ft-lb/in10 standard flex bars with 20 mil notch; ASTM D256
 0.520 J/cm
@Temperature -40.0 °C
0.974 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C153 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FASTM D648
Vicat Softening Point 79.0 °C174 °F1 kg load; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Haze 0.60 %0.60 %ASTM D1003
Gloss 171 %171 %at 60°; ASTM D 2457
Transmission, Visible 88 %88 %Regular transmittance per ASTM D 1003
 90 %90 %Total Transmittance; ASTM D 1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastar GN071 Natural PETG Copolyester
Eastman Eastar GN007 PETG Copolyester
Overview of materials for PETG Copolyester
Eastman Eastar 6763 PETG Copolyester
Eastman Eastar K3000 PETG Copolyester

PEA060 / 35226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.