MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: DuPont™ Neoprene 750 is an aqueous colloidal dispersion of a crystallization-resistant Neoprene. Its crystallization resistance is similar to that of DuPont™ Neoprene WRT. Neoprene 750 is anionic and is extremely stable with respect to shelf and heat aging. It immediately forms strong, highly extensible films when coagulated.

Main Features

  • Outstanding wet gels elongation and wet gel tensile strength render Neoprene 750 useful in dipped goods applications resist gel cracking either alone or in blends with other Neoprene liquid dispersion products such as DuPont™ Neoprene 571, or DuPont™ Neoprene 842A.
  • The low modulus of Neoprene 750 allows manufacture of very flexible products or dipped goods.

Neoprene 750 compounds without filler loading duplicate the lower stress/strain curve of similarly natural rubber latex products.

The high resistance to crystallization of Neoprene 750 allows it to maintain low modulus at relatively low temperatures regardless of the state of cure.

Suggested End Uses

  • Dipped goods
  • Contact bond adhesives
  • Cord adhesives
  • Construction adhesives

Denka Performance Elastomer LLC has acquired the Neoprene product line from DuPont Performance Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccLiquid Dispersion
 1.25 g/ccPolymer
Solids Content 50 %
pH >= 12
 
Descriptive Properties
ColorOff-white
Compounding StabilityGood
Emulsifying AgentPotassium salts
Freeze/Thaw StabilityNot stable
Mechanical StabilityGood
Storage StabilityGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Denka Neoprene 671A Polychloroprene
Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Denka Neoprene 571 Copolymer of chloroprene and sulfur
DuPont Mobility and Materials Neoprene 571 Polychloroprene

PDVC9800 / 170441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.