MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman Premi-Glas® 3101-20 Polyester BMC
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are:
  • Underwriters Laboratories, UL 94-5VA flame recognition at 2.6mm minimum thickness; and UL 94V-0 recognition at 1.6 mm minimum thickness; using halogen free technology.
  • Available in fiberglass content from 10-25%: standard product has 20% reinforcement.
  • Excellent dimensional stability, dielectric strength, and arc and track resistance.
  • Outstanding moldability and flow in Compression, Injection, and Transfer molding processes.
  • UL recognized in all colors. Standard color is black.

Data provided by Premix.

A. Schulman has acquired this former Premix product line.

Key Words: Bulk Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 1.95 g/cc1.80 - 1.95 g/cc
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm0.0015 - 0.0030 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 33.0 MPa4790 psiASTM D638
Tensile Modulus 13.0 GPa1890 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 10.3 GPa1490 ksiASTM D790
Poissons Ratio 0.300.30
Shear Modulus 5.00 GPa725 ksiCalculated
Izod Impact, Notched 4.25 J/cm7.96 ft-lb/inASTM D256
Izod Impact, Unnotched 5.30 J/cm9.93 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm457 kV/inASTM D149
Arc Resistance 210 sec210 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FASTM D792
UL RTI, Electrical 130 °C266 °FUL 746C
UL RTI, Mechanical with Impact 130 °C266 °FUL 746C
UL RTI, Mechanical without Impact 130 °C266 °FUL 746C
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 5VB
@Thickness 2.60 mm
5VB
@Thickness 0.102 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression, Transfer or Injection Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC
LG Chemical AF-325 ABS Resin
Plenco PlasGlas™ 40118 High Strength Glass Filled Thermoset Polyester BMC
Polynt 30 CF60- 6mm Carbon Fiber VE BMC
Polynt BMC 580 Bulk Molding Compound Green Compound With Natural Fiber

PPREMIX40 / 58189

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.