MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP825 Acrylic Adhesives
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and bond well to many metals, ceramics, wood and most plastics with minimal surface preparation.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity >= 3500 cPBase
 >= 7500 cPAccelerator
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Shear Strength 800 psiOverlap, Etched Aluminum tested after 1 week of Immersion in Toluene
 950 psiOverlap, Acrylic, Substrate Failure
 1000 psiOverlap, Etched Aluminum
 1025 psiOverlap, PC, Substrate Failure
 1050 psiOverlap, ABS, Substrate Failure
 1400 psiOverlap, PVC, Substrate Failure
 2175 psiOverlap, Etched Aluminum tested after 1 week of Immersion in 66°C tap water
 2525 psiOverlap, Etched Aluminum tested after 1 week of Immersion in Unleaded gasoline
 2600 psiOverlap, Cold-Rolled Steel - slightly oily, Cohesive Failure
 2625 psiOverlap, Green Fiberglass Reinforced Plastic, Adhesive Failure
 2625 psiOverlap, Etched Aluminum
 2675 psiOverlap, Etched Aluminum
 3025 psiOverlap, Cold-Rolled Steel - solvent cleaned, Adhesive Failure
 3825 psiOverlap, Etched Aluminum tested after 1 week of Immersion in IPA
 3850 psiOverlap, Aluminum - etched, Adhesive Failure
 3875 psiOverlap, Stainless Steel, Adhesive Failure
 3925 psiOverlap, Aluminum - abraded, 150 grit sandpaper, Adhesive Failure
 4100 psiOverlap, Aluminum - bare, Adhesive Failure
 4400 psiOverlap, Etched Aluminum tested after 1 week of Immersion in Diesel fuel
 4475 psiOverlap, Etched Aluminum
 4650 psiOverlap, Etched Aluminum tested after 1 week of Immersion in 50% Antifreeze
 4800 psiOverlap, Etched Aluminum cured for 7 days @ RT
 4850 psiOverlap, Etched Aluminum tested after 1 week of Immersion in 20% bleach solution
 6800 psiOverlap, Etched Aluminum tested after 1 week of Immersion in 66°C and 80% RH
Peel Strength 28.0 pliEtched Al/Etched Al after 1 week at RT cure
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 24.0 hourFull cure
 
Descriptive Properties
AppearanceOff-whiteBase
 Pale yellow
 YellowAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® HP Polyester Film, 36 Gauge
DuPont Teijin Films Mylar® ADS Polyester Film, 300 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 851H Polyester Film, 60 Gauge
3M Scotch-Weld™ DP820 Acrylic Adhesives

PMM34598 / 169345

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.