MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® 851H Polyester Film, 60 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® 851H (also called Mylar® 851) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallization, print, and lamination applications. This film is suitable for use in contact with food. Mylar® 851H has a thicker heat sealable layer than Mylar® 850H.

Approvals: FDA Food Contact Status - All gauges of Mylar® 851H (or Mylar® 851) comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® 851H (or Mylar® 851) can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Thickness 15.2 microns0.600 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 100 %100 %ASTM D882A
Film Elongation at Break, TD 90 %90 %ASTM D882A
Coefficient of Friction, Dynamic 0.500.50A-B; ASTM D1894
Coefficient of Friction, Static 0.600.60ASTM D1894
Film Tensile Strength at Break, MD 172 MPa25000 psiASTM D882A
Film Tensile Strength at Break, TD 186 MPa27000 psiASTM D882A
Heat Seal Strength Initiation Temperature 104 - 204 °C220 - 400 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Maximum Service Temperature, Air 121 °C250 °F
Shrinkage, MD 1.25 %
@Temperature 150 °C,
Time 1800 sec
1.25 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.30 %
@Temperature 150 °C,
Time 1800 sec
0.30 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
Haze 3.5 %3.5 %ASTM D1003
Transmission, Visible 88.6 %88.6 %TLT; ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)5 cc/100 in2O2, 24 hr; ASTM D1434 (77°F/75% RH/1 ATM)
Yield (nominal)33800 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® 850H Polyester Film, 80 Gauge
DuPont Teijin Films Mylar® 823 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 814 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge

PDTZ9271 / 139593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.