MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Features

Modified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, covers of electric tools. Complies with the 960°C glow wire and flammability grade V2. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccSTN 64 0111
Linear Mold Shrinkage 0.021 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0194 cm/cmSTN 64 0808
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPaSTN EN ISO 527-2
Elongation at Break 10 %STN EN ISO 527-2
Tensile Modulus 1300 MPaSTN EN ISO 527-2
Flexural Strength 35.0 MPaSTN EN ISO 178
Flexural Modulus 1200 MPaSTN EN ISO 178
Charpy Impact Unnotched 20.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 120 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 1.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 3.00 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmSTN IEC 60093
Surface Resistance 1.00e+16 ohmSTN IEC 60093
Dielectric Strength 24.0 kV/mmSTN IEC 60243
Comparative Tracking Index 450 VSTN 34 6468
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CSTN EN ISO 75/A
Vicat Softening Point 155 °CB; STN EN ISO 306
Flammability, UL94 V-2
Glow Wire Test 960 °CSTN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 30.0 - 50.0 °C
Injection Pressure 50.0 - 80.0 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLACO092 / 106970

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.