Features Modified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, covers of electric tools. Complies with the 960°C glow wire and flammability grade V2. Delivered in natural and in the full RAL color scale. Application: Injection Moulding Information Provided by Plastcom spol. s r.o. |