MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LATI LARFLEX 1882 PP/Elastomer Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polypropylene (PP)

Material Notes: Description: Larflex products are PP/Elastomer alloys. They are compounds designed especially for a good toughness and springback, even at low temperatures, and, unlike rubber, for an adequate rigidity at temperatures ranging between 60°C and 100°C. The Larflex series are mainly applied in the automotive sector, and in some cases, in equipment and machinery covers. They are therefore tough and feature good noise inertness, besides being fit for coloring when special methods are used. The Larflex compounds can be UV-stabilized for a better response to bad weather and solar light.

Specific Notes for this Material: excellent flowability; good surface finish; excellent impact resistance, even at low temperatures; suitable for external parts of all types of vehicles.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Water Absorption 0.020 %0.020 %at 23°C; ISO 62
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inLATI
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ASTM D785
Tensile Strength, Ultimate 26.0 MPa3770 psiISO 527
Flexural Modulus 0.870 GPa126 ksiASTM D790
Izod Impact, Notched  0.650 J/cm
@Temperature -40.0 °C
1.22 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.800 J/cm
@Temperature -20.0 °C
1.50 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 4.00 J/cm
@Temperature 23.0 °C
7.49 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  >= 30.0 J/cm²
@Temperature -20.0 °C
>= 143 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 >= 30.0 J/cm²
@Temperature -40.0 °C
>= 143 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 >= 30.0 J/cm²
@Temperature 23.0 °C
>= 143 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 24.0 kV/mm
@Thickness 2.00 mm
610 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C131 °FASTM D648
Vicat Softening Point 53.0 °C127 °F50°C/h 50N; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 220 °C392 - 428 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 - 100 °C176 - 212 °FFor thorough drying, use dehumidifiers or vacuum ovens. Temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourFor thorough drying, use dehumidifiers or vacuum ovens. Drying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)NIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet)
Polymax® Maxelast® P1870 TPE, PP Overmold or Standalone use
Polymax® Maxelast® P1740 TPE, PP Overmold or Standalone use
Overview of materials for Polypropylene, Molded
Overview of materials for Polycarbonate/PET Polyester Blend

PLATI171 / 50169

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.