MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zircar Ceramics SI-RIG Silica Rigidizer
Categories: Ceramic; Oxide; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Type SI-RIG Silica Rigidizer is a single part water based colloidal suspension of colloidal silica. It is principally used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic products, but is also widely used as a coating agent and binder.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³
Particle Size 0.020 µm0.020 µm
pH 9.39.3
Specific Surface Area 150 m²/g150 m²/g
Viscosity Measurement 20
@Temperature 25.0 °C
20
@Temperature 77.0 °F
no units given
 
Component Elements PropertiesMetricEnglishComments
Na2O 0.080 %0.080 %
SiO2 40 %40 %
 
Descriptive Properties
ColorWhite
Stabilizing IonAmmonium
Surface ChargeNegative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 316L Stainless Steel, annealed sheet
Titanium, Ti
Cadmium Polonide, CdPo
Aluminum Sulfide, Al2S3

CZIR012 / 2820

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.