MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Titanium Ti-4.5Al-3V-2Mo-2Fe (SP-700)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Characteristics: Alpha-beta alloy, beta-rich, fine microstructure, excellent superplastic formability.

Applications: Aerospace components, metal wood heads, metal balloons, tools, automotive components, wrist watch casings, mountain-climbing equipment.

Forms typically available: All mill product forms, also cast and powder metallurgy forms.

Mechanical properties values are for mill-annealed condition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 315
Tensile Strength >= 960 MPa
Tensile Strength, Yield >= 900 MPa
Elongation at Break >= 10 %
Tensile Modulus 110 GPa
Poissons Ratio 0.33
Shear Modulus 41.4 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000164 ohm-cm
Magnetic Permeability 1.0020
Magnetic Susceptibility 0.00000351cm3/g
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.71 µm/m-°C
@Temperature 25.0 - 100 °C
 8.53 µm/m-°C
@Temperature 25.0 - 300 °C
 8.95 µm/m-°C
@Temperature 25.0 - 500 °C
Specific Heat Capacity 0.495 J/g-°C
@Temperature 23.0 °C
 0.560 J/g-°C
@Temperature 400 °C
 0.660 J/g-°C
@Temperature 800 °C
Thermal Conductivity 7.00 W/m-K
@Temperature 23.0 °C
 10.0 W/m-K
@Temperature 400 °C
 19.0 W/m-K
@Temperature 800 °C
Melting Point 1593 °C
Beta Transus 900 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.0 - 5.0 %
Carbon, C <= 0.80 %
Hydrogen, H <= 0.010 %
Iron, Fe 1.7 - 2.3 %
Molybdenum, Mo 1.8 - 2.2 %
Niobium, Nb (Columbium, Cb) 6.5 - 7.5 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.15 %
Titanium, Ti 87 %
Vanadium, V 2.5 - 3.5 %
Yttrium, Y <= 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), STA
Titanium Ti-5Al-6Sn-2Zr-1Mo-0.25Si
Titanium Ti-8Mn, Annealed
Titanium Ti-5Al-2.5Fe ISO 5832/X Medical Grade
Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Beta Processed

MTP4322 / 142960

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.