Characteristics: Alpha-beta alloy, beta-rich, fine microstructure, excellent superplastic formability. Applications: Aerospace components, metal wood heads, metal balloons, tools, automotive components, wrist watch casings, mountain-climbing equipment. Forms typically available: All mill product forms, also cast and powder metallurgy forms. Mechanical properties values are for mill-annealed condition. |