MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID® 6/66 GF 15 GB 15 PA6/66 reinforced with glass fiber, glass beads  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/Nylon 6 Blend, Glass Fiber Filled

Material Notes: PA 6 and PA 66 alloy for injection molding, reinforced with 15% glass fiber and 15 % glass beads, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers of electric tools, automobile mirror housings, cooling screws of blowers, electromotors, bearing parts in the automotive industry. Delivered in natural mode and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccSTN EN ISO 1183-1
Filler Content 15 %Glass Beads
 15 %Glass Fibers
Linear Mold Shrinkage 0.0040 cm/cmSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmSTN EN ISO 294-4
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 275 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPaSTN EN ISO 527-2
Elongation at Break 3.5 %STN EN ISO 527-2
Tensile Modulus 5800 MPaSTN EN ISO 527-2
Flexural Strength 165 MPaSTN EN ISO 178
Flexural Modulus 4750 MPaSTN EN ISO 178
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 45.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 5.50 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CSTN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 245 °CSTN EN ISO 75-2 (A)
Vicat Softening Point 240 °CSTN EN ISO 306
Flammability, UL94 HB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
STN EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 80.0 °C
@Time 14400 sec
Moisture Content 0.10 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength
Plastcom SLOVAMID 66 GF 20 GF 10 PA66, 20% glass fibre, glass beads
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry

PPLACO534 / 140935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.