MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Material Notes:

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.70 %0.70 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
@Thickness 3.20 mm
0.0010 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
@Thickness 3.20 mm
0.0030 in/in
@Thickness 0.126 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ISO 2039
Tensile Strength at Break 240 MPa34800 psiISO 527-1/-2
Elongation at Break 1.8 %1.8 %ISO 527-1/-2
Tensile Modulus 19.0 GPa2760 ksiISO 527-1/-2
Flexural Strength 370 MPa53700 psiISO 178
Flexural Modulus 18.6 GPa2700 ksiISO 178
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179-1
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® C3 GF 60 1 black (4353) PA66 + PA6, Conditioned, 60% Glass Filled
BASF Ultramid® C3U10 PA6/66 FR (Conditioned)
Avient OnForce™ LFT NN-60 LGF/000 Natural Nylon 66 with 60% Long Glass Fiber
Avient Nymax™ GF 1200 60 Natural Nylon 66 with 60% Glass Fiber
Avient Nymax™ GF 1200 60 HS Natural A Nylon 66 with 60% Glass Fiber

PUNITIK863 / 177883

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.