MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: Feature: Injection Molding, Low Gloss, Heat Resistance

Application: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)

CAS No. 25120-20-1, 9003-56-9 and 25747-74-7

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 6.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 107ASTM D785
Tensile Strength, Yield 470 kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break 20 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Flexural Yield Strength 750 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Flexural Modulus 24000 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Izod Impact, Notched 24.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 27.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 12.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 13.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 101 °C
@Load 5.00 kg
50°C/h; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 30 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 200 - 220 °CInjection Molding
Middle Barrel Temperature 210 - 230 °CInjection Molding
Front Barrel Temperature 220 - 240 °CInjection Molding
Nozzle Temperature 220 - 240 °CInjection Molding
Melt Temperature 220 - 240 °CInjection Molding
Mold Temperature 40.0 - 60.0 °CInjection Molding
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 68.6 - 88.3 MPaInjection Molding
Screw Speed <= 80 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding
LG Chemical LG703W ABS, Low Gloss, Heat Resistance
LG Chemical LG-709 ABS, Low Gloss, Super High Heat Resistance
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding

PLAY051 / 148059

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.