MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LG703W ABS, Low Gloss, Heat Resistance
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: Feature: Injection Molding, Low Gloss, Heat Resistance

Application: Automobiles Interior Housing (Column Cover, Filllar Etc)

CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 9.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
9.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength, Yield 45.1 MPa
@Thickness 3.20 mm
6540 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 25 %
@Thickness 3.20 mm
25 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength 73.5 MPa
@Thickness 3.20 mm
10700 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.40 GPa
@Thickness 3.20 mm
348 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  1.96 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
3.67 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 2.45 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
4.59 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  0.883 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
1.65 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 0.981 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
@Thickness 6.40 mm
214 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
@Thickness 6.40 mm
198 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 99.0 °C
@Load 5.00 kg
210 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical 60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
UL RTI, Mechanical with Impact 60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
UL RTI, Mechanical without Impact 60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
 
Optical PropertiesMetricEnglishComments
Gloss 30 %30 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 200 - 220 °C392 - 428 °FInjection Molding
Middle Barrel Temperature 210 - 230 °C410 - 446 °FInjection Molding
Front Barrel Temperature 220 - 240 °C428 - 464 °FInjection Molding
Nozzle Temperature 220 - 240 °C428 - 464 °FInjection Molding
Melt Temperature 220 - 240 °C428 - 464 °FInjection Molding
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection Molding
Drying Temperature 70.0 - 80.0 °C158 - 176 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Back Pressure 68.6 - 88.3 MPa9950 - 12800 psiInjection Molding
Screw Speed <= 80 rpm<= 80 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
INEOS Styrolution Novodur® HH-106 ABS
LG Chemical BM662B ABS, Heat Resistance
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding

PLAY047 / 148055

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.