MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

Material Notes:
  • Features: Lubricated
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.69 g/ccMethod A; ASTM D792
Density 1.69 g/ccISO 1183
Linear Mold Shrinkage 0.0010 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaASTM D638
Tensile Strength, Yield 145 MPaASTM D638
Elongation at Break 1.7 %ASTM D638
Elongation at Yield 1.7 %ASTM D638
Tensile Modulus 12.3 GPaASTM D638
Flexural Strength 200 MPaASTM D790
Flexural Modulus 11.0 GPaASTM D790
Izod Impact, Notched 0.854 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Unnotched 5.50 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 9.40 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 26.4 kJ/m²ISO 180
Falling Dart Impact 3.40 JASTM D3763
Instrumented Impact Total Energy 1.97 JMulti-Axial Instrumented Impact Energy; ISO 6603-2
Coefficient of Friction, Dynamic 0.44vs. Steel - @ 40 psi, 50 ft/min, tested in accordance with LNP WI-0687; ASTM D1894
Coefficient of Friction, Static 0.35vs. Steel @ 40 psi, in accordance with LNP WI-0687; ASTM D1894
K (wear) Factor 33.0 x 10-10 in³-min/ft-lb-hr40psi, 50ft/min; tested in accordance with LNP WI-0687
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 269 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 316 - 321 °C
Mold Temperature 135 - 163 °C
Drying Temperature 121 - 149 °C
Dry Time 4 hour
Back Pressure 0.172 - 0.345 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
Lotte Advanced Materials Infino® XP-2165M PPS
Lotte Advanced Materials Infino® XP-2165BM PPS

PZLNP1165 / 51247

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.