MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes:
  • Features: Good Moldability
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.59 g/cc1.59 g/ccMethod A; ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 83.4 MPa12100 psiASTM D638
Elongation at Break 3.6 %3.6 %ASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 4.65 GPa674 ksiASTM D790
Izod Impact, Notched 0.374 J/cm
@Thickness 3.18 mm
0.701 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.80 J/cm
@Thickness 3.18 mm
8.99 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C397 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 354 - 371 °C669 - 700 °F
Mold Temperature 135 - 149 °C275 - 300 °F
Drying Temperature 121 - 149 °C250 - 300 °F
Dry Time 4 hour4 hour
Moisture Content 0.050 %0.050 %Suggested
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 101 NC010 PA66
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant

PZLNP1452 / 51534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.