MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 336.0-T65, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 336.0-T65; UNS A03360; AA336.0-T65; Al336.0-T65
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.72 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 110 - 140AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 157Estimated from Brinell Hardness.
Hardness, Rockwell A 47Estimated from Brinell Hardness.
Hardness, Rockwell B 77Estimated from Brinell Hardness.
Hardness, Vickers 143Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 40.0 ksiAA
Tensile Strength, Yield 296 MPa
@Strain 0.2 %
Elongation at Break 0.50 %in 50 mm
Tensile Modulus 73.0 GPaCompressive modulus in is typically about 2% higher for Al alloys
Compressive Yield Strength 296 MPa
Poissons Ratio 0.33
Machinability 30 %0-100 Scale (100=best)
Shear Modulus 30.0 GPa
Shear Strength 248 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000590 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/g
CTE, linear 19.8 µm/m-°C
@Temperature 20.0 - 100 °C
 21.6 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.963 J/g-°C
Thermal Conductivity 117 W/m-K
Melting Point 538 - 566 °C
Solidus 538 °C
Liquidus 566 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 1250 - 1500 °F
Solution Temperature 955 - 965 °Fhold at temperature 8 hr, cool in water at 150 to 212°F
Aging Temperature 335 - 345 °Fhold at temperature 12 - 26 hr; use solution heat-treated material
Casting Temperature 1250 - 1450 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 79 - 85.8 %As remainder
Copper, Cu 0.50 - 1.5 %
Iron, Fe <= 1.2 %
Magnesium, Mg 0.70 - 1.3 %
Manganese, Mn <= 0.35 %
Nickel, Ni 2.0 - 3.0 %
Other, each <= 0.05 %
Silicon, Si 11 - 13 %
Titanium, Ti <= 0.25 %
Zinc, Zn <= 0.35 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 336.0-T551, Permanent Mold Cast
336.1 Aluminum Composition Spec
Aluminum 333.0-F, Permanent Mold Cast
Aluminum 354.0-T62, Permanent Mold Cast
Aluminum 413.0-F Die Casting Alloy

MAC3360T65 / 9886

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.