MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Kanthal Super HT Molybdenum disilicide
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Kanthal Super HT is a electric heating element with outstanding properties for use at high temperatures, in air or oxygen, in cycling conditions. The maximum operating temperature is 1830°C (3330°F), and the element is suitable for furnace temperatures between 1500-1750°C (2730-3180°F) approximately. The special feature of Kanthal Super HT is the growth of the oxide layer the glaze is much reduced, compared to Kanthal Super 1800 and 1900. A thin oxide layer results in a much improved lifetime, because the tensions are reduced between the base material and the surrounding oxide, depending on the different thermal expansion coefficient. This is of great importance especially for elements of smaller dimensions used in cyclic conditions, where Kanthal Super 1800 and 1900 elements may be damaged by "banding". The banding effect is when the element shatters into smaller pieces during thermal cycling. This is a result of massive stresses between the oxide and the base material, once the oxide has grown to a sufficient thickness and the strength of the oxide film exceeds that of the base material. The new properties also include better hot strength and forms stability. Kanthal Super HT therefore, can be used in horizontal applications with less deformation although it still needs to be supported.

Special features

  • Lower oxidation rate
  • Thinner glaze layer
  • Longer life at high temperatures and when cycling
  • Less adhesion to fiber due to thinner glaze
  • Improved form stability
  • High purity - reduced Fe
  • Standard and specially designed elements
Typical applications for Kanthal Super HT includes laboratory and high temperature process furnaces and as a "problem solver" at high temperatures.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.00 g/cc0.253 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 75.0 - 125 MPa
@Temperature 1500 °C
10900 - 18100 psi
@Temperature 2730 °F
Elongation at Break 8.0 %8.0 %
Flexural Strength 350 - 400 MPa50800 - 58000 psi
Compressive Strength 1400 - 1500 MPa203000 - 218000 psi
Fracture Toughness 4.00 MPa-m½3.64 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 8.00 µm/m-°C3.89 - 4.44 µin/in-°F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity  15.0 W/m-K
@Temperature 600 - 1200 °C
104 BTU-in/hr-ft²-°F
@Temperature 1110 - 2190 °F
 30.0 W/m-K
@Temperature 20.0 - 600 °C
208 BTU-in/hr-ft²-°F
@Temperature 68.0 - 1110 °F
Maximum Service Temperature, Air 1800 °C3270 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.70 - 0.800.70 - 0.80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Ceramics AS-CEM Alumina-Silica Cement
Zircar Refractory Composites ZIRCAL-18 Refractory Board
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE
Zircar Ceramics HR-3M Dense Aluminum Oxide Support Rod

NSANDV5031 / 199595

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.