MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Refractory Composites ZIRCAL-18 Refractory Board
Categories: Ceramic

Material Notes: Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value makes it ideal for many fireproofing and heat processing equipment applications. ZIRCAL-18 is designed to serve as a backup insulation for any refractory construction, such as insulating fire brick, dense refractory brick, castable, gunning mix, plastic refractory or ceramic fiber.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.280 g/cc0.0101 lb/in³
Loss On Ignition 5.5 %5.5 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00110 GPa0.160 ksiparallel to thickness
Compressive Yield Strength 1.40 MPa203 psiat 5% deformation, parallel to thickness
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.10 µm/m-°C
@Temperature 20.0 - 700 °C
1.72 µin/in-°F
@Temperature 68.0 - 1290 °F
 5.50 µm/m-°C
@Temperature 20.0 °C
3.06 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity  0.0700 W/m-K
@Temperature 200 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 392 °F
parallel to thickness
 0.0900 W/m-K
@Temperature 400 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 752 °F
parallel to thickness
 0.100 W/m-K
@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1110 °F
parallel to thickness
Maximum Service Temperature, Air 1100 °C2010 °F
Shrinkage  0.00 %
@Temperature 650 °C,
Time 43200 sec
0.00 %
@Temperature 1200 °F,
Time 12.0 hour
Linear reheat (perpendicular to thickness)
 1.0 %
@Temperature 1050 °C,
Time 43200 sec
1.0 %
@Temperature 1920 °F,
Time 12.0 hour
Linear reheat (perpendicular to thickness)
 
Component Elements PropertiesMetricEnglishComments
Other 1.5 %1.5 %
 
Descriptive Properties
CaSiO3, %93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites RS-200 Refractory Sheet
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE
Crystex Composites Mykroy/Mycalex MM 1301 Molding Grade Glass-bonded Mica Composite

CZRCI11 / 2874

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.