MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Refractory Composites ZIRCAL-18 Refractory Board
Categories: Ceramic

Material Notes: Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value makes it ideal for many fireproofing and heat processing equipment applications. ZIRCAL-18 is designed to serve as a backup insulation for any refractory construction, such as insulating fire brick, dense refractory brick, castable, gunning mix, plastic refractory or ceramic fiber.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 g/cc
Loss On Ignition 5.5 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00110 GPaparallel to thickness
Compressive Yield Strength 1.40 MPaat 5% deformation, parallel to thickness
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.10 µm/m-°C
@Temperature 20.0 - 700 °C
 5.50 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.0700 W/m-K
@Temperature 200 °C
parallel to thickness
 0.0900 W/m-K
@Temperature 400 °C
parallel to thickness
 0.100 W/m-K
@Temperature 600 °C
parallel to thickness
Maximum Service Temperature, Air 1100 °C
Shrinkage 0.00 %
@Temperature 650 °C,
Time 43200 sec
Linear reheat (perpendicular to thickness)
 1.0 %
@Temperature 1050 °C,
Time 43200 sec
Linear reheat (perpendicular to thickness)
 
Component Elements PropertiesOriginal ValueComments
Other 1.5 %
 
Descriptive Properties
CaSiO3, %93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites RSLE-57 Refractory Sheet
Zircar Refractory Composites RS-200 Refractory Sheet
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE
Crystex Composites Mykroy/Mycalex MM 1301 Molding Grade Glass-bonded Mica Composite

CZRCI11 / 2874

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.