A general purpose series of low viscosity, strong, potting and encapsulating compounds. DI-PAK™ R-4525 has excellent electrical insulating properties and bonds well to many substrates. By varying the curing agents, the desired cure and working life can be obtained.Information provided by Hapco, Inc. |