Vacuum formed products are rigid, self-supporting fiber insulation manufactured from a slurry of ceramic fibers, binders and other proprietary ingredients. Customers are provided with optimized, engineered solutions from our wide range of formulations. Kaowool HP is a high strength product made from high purity fiber.Information provided by Morgan Advanced Materials |