MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical EM 40 Modified Glycerol Monotallate Surfactant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: EM 40 is a specially modified glycerol monotallate that is an oil soluble, non-ionic liquid surfactant. EM 40 is an excellent emulsifier for water in oil emulsions and can be used with hydrophilic emulsifiers to yield both oil in water and water in oil emulsions. EM 40 is soluble in many alcohols, aromatic and aliphatic hydrocarbons, but is insoluble in water. It is ashless and will not deposit a metallic film or stain metal subject to annealing or heat treated operations.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/cc
@Temperature 25.0 °C
Density 8.00 lb/gal
Saybolt Viscosity at 100°F 530 SUS
Saybolt Viscosity at 210°F 65 SUS
Kinematic Viscosity at 40°C (104°F) 100 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt
ASTM Color 3.0
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 5.0[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Pour Point <= 10.0 °F
 
Descriptive Properties
Theoretical HLB3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER135 / 217754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.