MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® BVOH Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Components: Butenediol vinyl alcohol copolymer based filament for Fused Filament Fabrication.

Product Description: Printing complex designs may only be possible with temporary support structures. Ultrafuse BVOH water-soluble support filament has been designed to easily dissolve in water. The solubility is increasing with higher water temperature. It offers great compatibility to a variety of materials: PLA, PRO1, ABS, ABS Fusion+, PA and PAHT CF15. Store this monofilament in a sealed bag or container to prevent moisture uptake.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.138 g/cc0.04111 lb/in³Printed Part; ISO 1183-1
Melt Flow 12.9732 g/10 min
@Load 2.16 kg,
Temperature 210 °C
12.9732 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 8.70 MPa1260 psiZX: Upright; ISO 527
 33.7 MPa4890 psiXY: Flat; ISO 527
Elongation at Break 0.60 %0.60 %ZX: Upright; ISO 527
 14.8 %14.8 %XY: Flat; ISO 527
Modulus of Elasticity 1.426 GPa206.8 ksiYoung's, ZX: Upright; ISO 527
 2.339 GPa339.2 ksiYoung's, XY: Flat; ISO 527
Flexural Strength 11.4 MPa1650 psiZX: Upright; ISO 178
 50.3 MPa7300 psiXZ: On its edge; ISO 178
 53.8 MPa7800 psiXY: Flat; ISO 178
Flexural Modulus 1.081 GPa156.8 ksiZX: Upright; ISO 178
 1.807 GPa262.1 ksiXZ: On its edge; ISO 178
 2.236 GPa324.3 ksiXY: Flat; ISO 178
Flexural Strain at Break 1.0 %1.0 %ZX: Upright; ISO 178
 4.4 %4.4 %XZ: On its edge; ISO 178
 4.8 %4.8 %XY: Flat; ISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 °C347 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 122 °C252 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 100 °C140 - 212 °FBed, Bed Material: PC adhesive
Nozzle Temperature 190 - 210 °C374 - 410 °F
Drying Temperature 60.0 °C140 °Fin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour4.00 - 16.0 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed30-60 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D021 / 312262

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.