MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, variable ratio, a viscosity of 300 cps., and a weight of 7.8 lbs/gallon. AboCast 7802-1/AboCure 7804-3 has versatility, many variable-ratio possibilities, and a tenacious adhesion to metals, ceramics, glass, wood, and most rigid materials which permits permanent structural and dielectric bonds. Absence of volatiles and minimum shrinkage, typical of solventless epoxy systems, allow castings and masses of virtually any desired thickness. Suggested Uses: Multi-purpose casting, coating, and bonding for applications requiring high dielectric resistance, structural strength, and radiation resistance as well as resistance to weather, water, alkalis, diluted acids, fuels, and most common solvents; it was originally developed for FERMILAB.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 lb/galAboCure 7804-3
 9.10 lb/galAboCast 7802-1
Water Absorption 0.20 - 0.40 %
Viscosity 350 - 500 cPblended
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 25
@Time 86400 sec
1/8 in thickness
 40
@Time 259000 sec
1/8 in thickness
 50
@Time 86400 sec
 60
@Time 259000 sec
 60
@Treatment Temp. 100 °C,
Time 10800 sec
 60
@Treatment Temp. 100 °C,
Time 10800 sec
1/8 in thickness
Tensile Strength at Break 2000 - 4000 psi
Elongation at Break >= 20 %
Flexural Strength 2000 - 3000 psi
Compressive Strength 3000 - 4000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 300 - 400 V/mil
 
Processing PropertiesOriginal ValueComments
Pot Life 120 min100 g
 
Descriptive Properties
Parts by Weight (pbw)100AboCast 7802-1
 80AboCure 7804-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab® EP1385 Clear Epoxy Formulation
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Henkel Loctite® 5072 Silicone Chip Coating
Henkel Loctite® 3532 High viscosity Dam Encapsulant

PABC828 / 107812

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.