MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SCG Chemicals EL-Pro™ P701J Polypropylene Injection Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Key Characteristics:
  • High stiffness
  • High gloss
  • High productivity
  • Good processability
  • Odorless
  • Safe for food contact

Recommended Applications:

  • General purpose housewares
  • Food containers
  • Medical instruments
  • Infant articles, toys
  • Office accessories

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D1505
Linear Mold Shrinkage, Flow 0.012 cm/cm
@Thickness 2.00 mm
TPE Method
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Thickness 2.00 mm
TPE Method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D785
Tensile Strength at Break 20.0 MPaASTM D638
Tensile Strength, Yield 320 kg(f)/cm²ASTM D638
Elongation at Break 650 %ASTM D638
Flexural Modulus 15500 kg(f)/cm²ASTM D790
Izod Impact, Notched 2.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 2.00 kg-cm/cm
@Temperature 0.000 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
Vicat Softening Point 155 °CASTM D1525
Brittleness Temperature -20.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 47 %
@Thickness 1.00 mm
ASTM D1003
Gloss 51 %
@Thickness 1.00 mm
ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H6105JU High Density Polyethylene Injection Molding
Multibase Multi-Pro® 1012 C Polypropylene
LyondellBasell Hostacom™ TKS709D Thermoplastic Polyolefin Elastomer
LyondellBasell Hostacom™ CB275FC Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ HSBMG265 Thermoplastic Polyolefin Elastomer

PSCGC963 / 120717

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.