MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom™ CB275FC Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hostacom™ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, rigidity and impact and scratch and mar resistance. It was designed for automotive interior components that must have a very good impact/stiffness balance such as instrument panels or other componentry that require compliance to FMVSS201 or FMVSS208. Uses: Automotive interior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 230 °C
17 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7272ISO 2039-2
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1, -2
Elongation at Break 200 %200 %ISO 527-1, -2
Flexural Modulus 1.90 GPa276 ksiISO 178
Izod Impact, Notched (ISO)  3.90 kJ/m²
@Temperature -30.0 °C
1.86 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 41.0 kJ/m²
@Temperature 23.0 °C
19.5 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C234 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C135 °FUnannealed; ISO 75A-1, -2
Shrinkage 1.0 %1.0 %Tool, 100x150x3.2 mm; Basell Test Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Entec Hypel® PEHD.7/.962 HDPE
LyondellBasell Hostacom™ CB271FC Thermoplastic Polyolefin Elastomer
LyondellBasell Astryn 6652 Polypropylene Homopolymer
Ineos T60-500 HDPE
Hyosung Topilene HJ740 PP

PMO820 / 53809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.