MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fibre Glast 99 Clear Polyester Casting Resin  (discontinued **)
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Description:

#99 Clear Casting Resin is ideal for poured castings. Larger castings have been achieved through multiple pours and slight catalyst adjustments. It may be used with colored pigments for opaque castings. The resin exhibits extremely low shrinkage when catalyzed at 1/2% MEKP. #99 is a low viscosity, low reactivity, orthophthalic polyester. It is prepromoted for curing with various methyl ethyl ketone peroxides (MEKPs) #69.

Features:
  • Low shrinkage
  • Low viscosity
  • UV Stabilized
  • Specially promoted

Benefits:
  • Minimal warping
  • Outstanding air release
  • Meets California Rule 50 and SCAQMD 1162
  • Resists yellowing
  • Water white when cured
  • Designed for small or large castings

Properties are typical for 1/8" Clear Casting at room temperature of 77°F

Suggested Uses:Decorative castings, tabletops, art objects and biological encapsulations.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 3737ASTM D2583
Tensile Strength at Break 68.9 MPa10000 psiASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 71.0 °C160 °FDeflection Temp; Load not specified; ASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Gel Time 14.0 - 20.0 min14.0 - 20.0 min
 
Descriptive Properties
Maximum Exotherm300°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)
Polynt POLYCOR® GPLY 4000-022 Neutral Isophthalic Brush Gel Coat
Polynt POLYCOR® GPLY 3000-122 White Pigmented Isophthalic Brush Gel Coat
Polynt POLYCOR® GPLY 1000-121 White Pigmented Isophthalic Spray Gel Coat
Polynt POLYCOR® 944 Series Isophthalic Gel Coat

PFIBRE34 / 38298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.