MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® GPLY 1000-121 White Pigmented Isophthalic Spray Gel Coat
Categories: Polymer; Thermoset

Material Notes: Appearance: White, thixotropic liquid.

Isophthalic gel coat, Medium reactivity, Accelerated, Light stabilized.

Application: Sanitary, marine, etc.…

Characteristics: Medium chemical resistance, Medium heat resistance, Resilient.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 12000 - 16000 cP12000 - 16000 cPRVF, Spindle No.4 @ 4 rpm
 
Processing PropertiesMetricEnglishComments
Gel Time 12.0 - 15.0 min
@Temperature 25.0 °C
12.0 - 15.0 min
@Temperature 77.0 °F
Reactivity at 25°C, using 1.8% MEKP-925
 
Descriptive Properties
Thixotropic Index6-7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polynt POLYCOR® GPLY 4000-022 Neutral Isophthalic Brush Gel Coat
Polynt POLYCOR® GPLY 3000-122 White Pigmented Isophthalic Brush Gel Coat
Polynt POLYCOR® 944 Series Isophthalic Gel Coat
Fibre Glast 99 Clear Polyester Casting Resin
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)

PPOLYN9240 / 231835

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.