MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kohesi Bond KB 1040 Two component, room temperature curing clear epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Phenomenal optical clarity
  • Excellent flow properties
  • Outstanding adhesion to various substrates
  • Very low shrinkage post curing
  • Exceptional electrical insulation
  • Stellar dimensional stability
Kohesi Bond KB 1040 is a two component, room temperature curing epoxy system suitable for bonding, sealing, potting and encapsulation. It has a favorable 4:1 (Part A: Part B) mix ratio by weight. This epoxy system offers excellent adhesion to a variety of substrates, such as metals, glass, ceramics, most plastics and rubbers. It readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 1 - 2 hours. KB 1040 is optically clear and offers top notch light transmissions properties. It has a refractive index of 1.57. It offers an extensive service temperature range of -50°C to +120°C. This adhesive fosters outstanding physical strength properties as well as dimensional stability. It offers minimal shrinkage upon cure. This makes it suitable for gap filling applications. It also offers excellent chemical resistance to a variety of fuels, oils, acids, bases and water. Part A is clear in color and Part B is light straw in color. KB 1040 is widely used in optical, optoelectronic, fiber-optic, electronics, aerospace and related industries especially when optical clarity is desirable.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 250 - 500 cP250 - 500 cPPart B
 400 - 1000 cP400 - 1000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength >= 68.9 MPa>= 10000 psi
Tensile Modulus >= 2.83 GPa>= 410 ksi
Adhesive Bond Strength >= 22.1 MPa>= 3200 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 3.56
@Frequency 60 Hz
3.56
@Frequency 60 Hz
Dielectric Strength 17.3 kV/mm
@Thickness 3.17 mm
440 kV/in
@Thickness 0.125 in
Dissipation Factor 0.0050
@Frequency 60 Hz
0.0050
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 90.0 °C
2.00 - 3.00 hour
@Temperature 194 °F
Option 2
 1440 - 2880 min
@Temperature 23.0 °C
24.0 - 48.0 hour
@Temperature 73.4 °F
Option 1
Working Life 25.0 - 40.0 min25.0 - 40.0 min100 g of mixed epoxy
Shelf Life 12.0 Month12.0 Monthin original unopened containers
 
Descriptive Properties
Mixing Ratio4:1 by weightPart A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI920 / 249099

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.