MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Powersil® 3500 MH Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: HTV silicone rubber POWERSIL® 3500 MH is an addition-curing one-component compound for the manufacture of press cured articles. The vulcanizates are tracking resistant and show good to very good mechanical properties. No peroxide split products are released during cure or post cure. Cure system is significantly faster compared to peroxide curing materials. Cure time is reduced to 30 - 50 % depending on the wall thickness.

Special features:

    easy demolding
  • dry surface
  • no unpleasant smell caused by peroxides
  • no inhibition by oxygen
  • excellent dielectric properties
  • high arcing and tracking resistance
Application: The grade is suitable for the manufacture of articles like cable accessories e. g. joints, terminations or single sheds for outdoor applications. Specially thick walled articles can take advantage of the fast curing material.
  • outdoor or indoor cable terminations
  • silicone sheds

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183-1 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ISO 868
Tensile Strength at Break 10.0 MPa1450 psiISO 37
Elongation at Break 850 %850 %ISO 37
Tear Strength 30.0 kN/m171 pliASTM 624 B
Compression Set 20 %
@Temperature 175 °C,
Time 79200 sec
20 %
@Temperature 347 °F,
Time 22.0 hour
ISO 1653
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.92.9IEC 60250
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243
Dissipation Factor 0.000500.00050IEC 60250
Arc Resistance >= 300 sec>= 300 secIEC 61621
 
Descriptive Properties
Colorred
Track Resistance> 3.5 kV/6hIEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9386 / 204915

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.