MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones LIMS™ KE1950-30A/B Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: KE-1950-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy pumping through most injection molding systems.

    Features
  • Rapid cure time at elevated temperature
  • Long pot life at room temperature

    Applications
  • O-rings
  • Diaphragms
  • Capping
  • Rubber rollers
  • Connector packings
  • Other electrical parts

Information Provided by Shin-Etsu Silicones of America, Inc.

Key Words: LSR, Liquid Silicone Rubber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 250000 cPA
 250000 cPB
Linear Mold Shrinkage 0.020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 32
Tensile Strength 8.80 MPa
Elongation at Yield 700 %
100% Modulus 0.101 ksi
@Strain 100 %
Tear Strength 25.0 kN/m
Compression Set 6.0 %
@Temperature 200 °C,
Time 14400 sec
 22 %
@Temperature 150 °C,
Time 3600 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 120 °C
Press Cure
 60.0 min
@Temperature 150 °C
Post Cure
 
Compliance PropertiesOriginal ValueComments
FDA Yes
USP Class VI Yes
 
Descriptive Properties
AppearanceTranslucent
Cure Rate29T10 (302°F, ODR)
 39T90 (302°F, ODR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones LIMS™ KE1950-10A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-20A/B Elastomer
Overview of materials for Silicone Rubber
Shin-Etsu Silicones KEG-2000-30A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-35A/B Elastomer

PSHIN003 / 103830

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.