MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Shin-Etsu Silicones LIMS™ KE1950-10A/B Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy pumping through most injection molding systems.

    Features
  • Rapid cure time at elevated temperature
  • Long pot life at room temperature

    Applications
  • O-rings
  • Diaphragms
  • Capping
  • Rubber rollers
  • Connector packings
  • Other electrical parts

Information Provided by Shin-Etsu Silicones of America, Inc.

Key Words: LSR, Liquid Silicone Rubber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Viscosity 60000 cP60000 cPA
 60000 cP60000 cPB
Linear Mold Shrinkage 0.023 cm/cm0.023 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1313
Tensile Strength 3.90 MPa566 psi
Elongation at Yield 700 %700 %
100% Modulus 0.207 MPa
@Strain 100 %
30.0 psi
@Strain 100 %
Tear Strength 10.0 kN/m57.1 pli
Compression Set  8.0 %
@Temperature 200 °C,
Time 14400 sec
8.0 %
@Temperature 392 °F,
Time 4.00 hour
 12 %
@Temperature 150 °C,
Time 3600 sec
12 %
@Temperature 302 °F,
Time 1.00 hour
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 120 °C
0.0833 hour
@Temperature 248 °F
Press Cure
 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Post Cure
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
USP Class VI YesYes
 
Descriptive Properties
AppearanceTranslucent
Cure Rate38T10 (302°F, ODR)
 86T90 (302°F, ODR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones LIMS™ KE1950-20A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-60A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-50A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-70A/B Elastomer
Shin-Etsu Silicones LIMS™ KE1950-30A/B Elastomer

PSHIN001 / 103828

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.