VTM264FRB is a black, flame-retarded, controlled flow epoxy resin matrices systems with a broad 65 to 120°C (150 to 250°F) processing window, offering low temperate initial cures or reduced total cycle times. VTM264FRB and VTM267FRB are formatted for a range of low cost, vacuum-bag pressure, composite molding processes, including ZPREG partial impregnation technology. VTM267FRB offers enhanced workshop handling characteristics with and controlled tack for sided impregnation and film infusion processing with heavy reinforcements. Features & Benefits: - Open vacuum bag curing
- 21 days out life 21°C (70°F)
- 12 months storage at -18°C (0°F)
- Self-extinguishing to FMVSS30/ISO3795/SAE J369
- Flexible cure between 65 at 120°C (149 and 248°F)
- Minimum initial cure temperature 65°C (149°F)
- Maximum dry service temperature of 100°C (212°F) following suitable post-cure
- Excellent tack and drape for easy lay-up of large structures, vertical surfaces and complex shapes
- VTM267FRB offers controlled tack for sided impregnation and film infusion processing
- Compatible with all VTM260 and ZPREG260 series materials
Note 1: Cure cycle: 1 hr at 120°C (248°F), 6.2 bar (90 psi)Information provided by Cytec, subsequently acquired by Solvay. |