MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, even in the dry state, good heat-ageing resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 7.0 %7.0 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 2.0 %2.0 %23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number 134 cm³/g1.34 dl/gISO 307, 1157, 1628
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 260 °C
15 g/10 min
@Load 11.0 lb,
Temperature 500 °F
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiConditioned; ISO 527-1/-2
 160 MPa23200 psiISO 527-1/-2
Elongation at Break 4.0 %4.0 %ISO 527-1/-2
 7.0 %7.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 5.20 GPa754 ksiConditioned; ISO 527-1/-2
 9.00 GPa1310 ksiISO 527-1/-2
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 2.80 J/cm²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Puncture Energy 10.0 J7.38 ft-lbISO 6603-2
 15.0 J11.1 ft-lbConditioned; ISO 6603-2
 7.00 J
@Temperature -30.0 °C
5.16 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 7.00 J
@Temperature -30.0 °C
5.16 ft-lb
@Temperature -22.0 °F
Conditioned; ISO 6603-2
Tensile Creep Modulus, 1 hour 4200 MPa609000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 3300 MPa479000 psiISO 899-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Melting Point 213 °C415 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 90.0 °C194 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
Oxygen Index 22 %22 %ISO 4589-1/-2
 
Descriptive Properties
FeaturesHeat stabilized or stable to heat
 High impact or high impact modified
FormPellets
ISO Short NameISO 1874-PA 6/66-I, MHR, 14-090, GF30
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 130 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Polyether Block Amide (PEBA)
Envalior Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Dry

PLANX0746 / 98961

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.