MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Overview of materials for Polymethylpentene, Molded
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP); Polymethylpentene, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.833 - 0.913 g/ccAverage value: 0.847 g/cc Grade Count:11
Water Absorption 0.0100 - 0.100 %Average value: 0.0190 % Grade Count:10
Water Vapor Transmission 46.5 - 46.5 g/m²/day
@Temperature 37.8 - 37.8 °C
Average value: 46.5 g/m²/day Grade Count:1
Linear Mold Shrinkage 0.0150 - 0.0300 cm/cmAverage value: 0.0176 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.0120 cm/cmAverage value: 0.0120 cm/cm Grade Count:4
Melt Flow 9.00 - 110 g/10 minAverage value: 54.6 g/10 min Grade Count:7
Spiral Flow 50.0 - 56.0 cmAverage value: 52.0 cm Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 42.0 - 91.0Average value: 74.7 Grade Count:7
Tensile Strength, Ultimate 10.0 - 30.0 MPaAverage value: 23.3 MPa Grade Count:11
Tensile Strength, Yield 20.0 - 30.0 MPaAverage value: 27.3 MPa Grade Count:8
Elongation at Break 10.0 - 60.0 %Average value: 19.4 % Grade Count:11
Modulus of Elasticity 0.820 - 1.93 GPaAverage value: 1.63 GPa Grade Count:11
Flexural Yield Strength 21.0 - 47.0 MPaAverage value: 38.4 MPa Grade Count:10
Flexural Modulus 0.630 - 1.60 GPaAverage value: 1.34 GPa Grade Count:11
Izod Impact, Notched 0.200 - 0.534 J/cmAverage value: 0.272 J/cm Grade Count:8
Izod Impact, Unnotched (ISO) 8.00 - 129 kJ/m²Average value: 43.0 kJ/m² Grade Count:7
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10200 - 1.00e+16 ohm-cmAverage value: 8.89e+15 ohm-cm Grade Count:9
Dielectric Constant 2.10 - 2.12Average value: 2.10 Grade Count:8
Dielectric Strength 65.0 - 146 kV/mmAverage value: 75.1 kV/mm Grade Count:8
 
Thermal PropertiesOriginal ValueComments
CTE, linear 117 µm/m-°CAverage value: 117 µm/m-°C Grade Count:7
Melting Point 223 - 235 °CAverage value: 231 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 127 °CAverage value: 115 °C Grade Count:9
Vicat Softening Point 147 - 180 °CAverage value: 169 °C Grade Count:7
Flammability, UL94 HBGrade Count:3
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46 - 1.46Average value: 1.46 Grade Count:8
Haze 0.800 - 2.10 %Average value: 1.52 % Grade Count:8
Transmission, Visible 93.0 - 94.0 %Average value: 93.4 % Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene
Overview of materials for Polypropylene, Molded
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade

O4290 / 78309

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.