MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Polymethylpentene, Molded
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP); Polymethylpentene, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.833 - 0.913 g/cc0.0301 - 0.0330 lb/in³Average value: 0.847 g/cc Grade Count:11
Water Absorption 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0190 % Grade Count:10
Water Vapor Transmission 46.5 - 46.5 g/m²/day
@Temperature 37.8 - 37.8 °C
2.99 - 2.99 g/100 in²/day
@Temperature 100 - 100 °F
Average value: 46.5 g/m²/day Grade Count:1
Linear Mold Shrinkage 0.0150 - 0.0300 cm/cm0.0150 - 0.0300 in/inAverage value: 0.0176 cm/cm Grade Count:6
Linear Mold Shrinkage, Transverse 0.0120 cm/cm0.0120 in/inAverage value: 0.0120 cm/cm Grade Count:4
Melt Flow 9.00 - 110 g/10 min9.00 - 110 g/10 minAverage value: 54.6 g/10 min Grade Count:7
Spiral Flow 50.0 - 56.0 cm19.7 - 22.0 inAverage value: 52.0 cm Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 42.0 - 91.042.0 - 91.0Average value: 74.7 Grade Count:7
Tensile Strength, Ultimate 10.0 - 30.0 MPa1450 - 4350 psiAverage value: 23.3 MPa Grade Count:11
Tensile Strength, Yield 20.0 - 30.0 MPa2900 - 4350 psiAverage value: 27.3 MPa Grade Count:8
Elongation at Break 10.0 - 60.0 %10.0 - 60.0 %Average value: 19.4 % Grade Count:11
Modulus of Elasticity 0.820 - 1.93 GPa119 - 280 ksiAverage value: 1.63 GPa Grade Count:11
Flexural Yield Strength 21.0 - 47.0 MPa3050 - 6820 psiAverage value: 38.4 MPa Grade Count:10
Flexural Modulus 0.630 - 1.60 GPa91.4 - 232 ksiAverage value: 1.34 GPa Grade Count:11
Izod Impact, Notched 0.200 - 0.534 J/cm0.375 - 1.00 ft-lb/inAverage value: 0.272 J/cm Grade Count:8
Izod Impact, Unnotched (ISO) 8.00 - 129 kJ/m²3.81 - 61.4 ft-lb/in²Average value: 43.0 kJ/m² Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10200 - 1.00e+16 ohm-cm10200 - 1.00e+16 ohm-cmAverage value: 8.89e+15 ohm-cm Grade Count:9
Dielectric Constant 2.10 - 2.122.10 - 2.12Average value: 2.10 Grade Count:8
Dielectric Strength 65.0 - 146 kV/mm1650 - 3710 kV/inAverage value: 75.1 kV/mm Grade Count:8
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C65.0 µin/in-°FAverage value: 117 µm/m-°C Grade Count:7
Melting Point 223 - 235 °C433 - 455 °FAverage value: 231 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 127 °C176 - 261 °FAverage value: 115 °C Grade Count:9
Vicat Softening Point 147 - 180 °C297 - 356 °FAverage value: 169 °C Grade Count:7
Flammability, UL94 HBHBGrade Count:3
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46 - 1.461.46 - 1.46Average value: 1.46 Grade Count:8
Haze 0.800 - 2.10 %0.800 - 2.10 %Average value: 1.52 % Grade Count:8
Transmission, Visible 93.0 - 94.0 %93.0 - 94.0 %Average value: 93.4 % Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene
Overview of materials for Polypropylene, Molded
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade

O4290 / 78309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.